Print settings

Nozzle temperature (°C)
190–240Source: [1][2][3]
Hardened nozzle
Not requiredSource: [1][2][3]
Cool plate (°C)
35–45Source: [1][2][3]
Engineering plate (°C)
45–65 (glue required)Source: [1][2][3]
Smooth PEI (°C)
45–65Source: [1][2][3]
Textured PEI (°C)
45–65Source: [1][2][3]
Open-frame printer
CompatibleSource: [1][2][3]
Enclosed printer
CompatibleSource: [1][2][3]
AMS
CompatibleSource: [1][2][3]
0.2 mm nozzle
CompatibleSource: [1][2][3]
0.4 mm nozzle
CompatibleSource: [1][2][3]
0.6 mm nozzle
CompatibleSource: [1][2][3]
0.8 mm nozzle
CompatibleSource: [1][2][3]
0.4 HF mm nozzle
CompatibleSource: [1][2][3]
0.6 HF mm nozzle
CompatibleSource: [1][2][3]
0.8 HF mm nozzle
CompatibleSource: [1][2][3]

Density and drying

Published densities

Drying

Recommended before printing. Source: [1][2][3]

Drying methods from the source table
MethodSettingSource note
AMS 2 Pro45°C, 12hSource: [1][2][3]—
AMS HT45°C, 12hSource: [1][2][3]—
AMS 3H55°C, 12hSource: [1][2][3]—
Convection oven50°C, 8hSource: [1][2][3]—
Printer heatbed (H, X, P1S, P2S)60–70°C, 12hSource: [1][2][3]—

Flip: Every 6 hoursSource: [1][2][3]

Cover: Filament packaging box or PC boxSource: [1][2][3]

Notes

  • Bambu's guide says PLA is not recommended for parts that sit at about 50 °C or higher.Source: [1][2][3]
  • Drying values shown are the PLA Basic / PLA Matte row; PLA Silk and PLA Aero have their own rows in the source.Source: [1][2][3]

Sources

Numbered markers beside values link to the source documents for this record.

  1. [1] Bambu Lab Wiki: Filament guide (printer, nozzle, AMS, build plate)
  2. [2] Bambu Lab Wiki: Filament drying guide
  3. [3] BambuStudio filament profiles on GitHub (filament_density)